MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Silpuran® 2450 A/B Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Addition-curing RTV-2 silicone rubber curing to a silicone elastomer of high hardness.

Properties :

  • Highly biocompatible
  • No by-products from curing process
  • Pourable after stirring
  • 2-part, mixing ratio 1 : 1
  • Rapid curing at relatively low temperatures
  • White to slightly grayish vulcanizate with hardness of Shore A 50
Application: SILPURAN® 2450 A/B can be used for flexible molding applications in prosthetics.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³Component B; DIN EN ISO 2811
 1.30 g/cc0.0470 lb/in³cured
 1.38 g/cc0.0499 lb/in³Component A; DIN EN ISO 2811
Viscosity  20000 cP
@Shear Rate 10.0 1/s
20000 cP
@Shear Rate 10.0 1/s
Component B; DIN EN ISO 3219
 35000 cP
@Shear Rate 10.0 1/s
35000 cP
@Shear Rate 10.0 1/s
Component A; DIN EN ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050ISO 868
Tensile Strength at Break 6.00 MPa870 psiISO 37
Elongation at Break 200 %200 %ISO 37
Tear Strength 7.00 kN/m39.9 pliASTM D624B
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Treatment Temp. 135 °C
0.167 hour
@Treatment Temp. 275 °F
Pot Life 45.0 - 60.0 min45.0 - 60.0 min
 
Descriptive Properties
Colorslightly greyishComponent A
 slightly greyishComponent B
 white to slightly greyishCatalyzed A+B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow HV 1650/50 SILICONE RUBBER
Trelleborg Commercial Neoprene® C500 Chloroprene
Trelleborg Commercial Neoprene® C400 Chloroprene
Wacker Elastosil® R 701/50 Silicone Rubber
Wacker Elastosil® LR 3004/50 A/B Liquid Silicone Rubber

PWACK9482 / 205011

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.