Addition-curing RTV-2 silicone rubber curing to a silicone elastomer of high hardness. Properties : - Highly biocompatible
- No by-products from curing process
- Pourable after stirring
- 2-part, mixing ratio 1 : 1
- Rapid curing at relatively low temperatures
- White to slightly grayish vulcanizate with hardness of Shore A 50
Application: SILPURAN® 2450 A/B can be used for flexible molding applications in prosthetics.Information provided by Wacker Chemie AG. |