MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Petrochemical Ravathane® R210A93UV Ether-Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: UV stabilized. Typical properties: excellent abrasion and scratch resistance, high elasticity, high tensile & tear strength, good oil and grease resistnace, low temperature flexibility, recyclable, adhesion to polar substrates. Applications: Shoe soles, tactile markers, castor wheels, delinetors, hose & tubing, timing belt, animal identification tags.

Information provided by Ravago Petrokimya (Ravago Petrochemical).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 11831-A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ISO 868
Tensile Strength 40.0 MPa5800 psiISO 37
Elongation at Break 590 %590 %ISO 37
100% Modulus 10.0 MPa
@Strain 100 %
1450 psi
@Strain 100 %
ISO 37
300% Modulus 17.0 MPa
@Strain 300 %
2470 psi
@Strain 300 %
ISO 37
Izod Impact, Notched (ISO)  32.0 kJ/m²
@Temperature -30.0 °C
15.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Izod Impact, Unnotched (ISO)  42.0 kJ/m²
@Temperature -30.0 °C
20.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Tear Strength 130 kN/m742 pliISO 34-1/B/b
Abrasion 4040mm3; ISO 4649
Compression Set  20 %
@Temperature 23.0 °C,
Time 79200 sec
20 %
@Temperature 73.4 °F,
Time 22.0 hour
ISO 815-1
 40 %
@Temperature -30.0 °C,
Time 79200 sec
40 %
@Temperature -22.0 °F,
Time 22.0 hour
ISO 815-1
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Vicat Softening Point 110 °C230 °FISO 306-A
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 185 - 200 °C365 - 392 °F
Moisture Content <= 0.10 %<= 0.10 %Drying is important

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane
NEU NEUSoft™ 455-50A Ester/ether TPU / SBC blend
RTP Company RTP 1200 T-70A UV Ether-based Thermoplastic Polyurethane Elastomer (; UV Stabilized

PRAVAGO919 / 198209

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.