MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyPLASTY PolyPET PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Great mechanical strength, excellent dimensional stability (better than POM), abrasion resistance and very good shear properties. Good electrical properties; it is physiologically acceptable and flame retardant. It has very low water absorption, which does not affect its mechanical and electrical properties. Its very low thermal expansion coefficient puts it among the leading thermoplastics. This material is easily glued and welded.

Information provided by PolyPLASTY.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Water Absorption 0.20 %0.20 %under regular conditions; ISO 62
Moisture Absorption at Equilibrium 0.50 %0.50 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, H358/30 150 MPa21800 psiISO 2039-1
Hardness, Shore D 8383ISO 868, ISO 2039-2
Tensile Strength, Yield 80.0 MPa11600 psiISO 527
Elongation at Break 70 %70 %ISO 527
Modulus of Elasticity 2.80 GPa406 ksiISO 527
Fatigue Strength 31.0 MPa4500 psiflexure; ASTM D671
Izod Impact, Notched 0.200 J/cm0.375 ft-lb/inISO 180/4A
Tensile Creep Modulus, 1000 hours 2000 MPa290000 psi0.5 percent; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohm6.00e+14 ohmIEC 60093
Dielectric Constant  3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
 3.4
@Frequency 50 Hz
3.4
@Frequency 50 Hz
IEC 60250
Dielectric Strength 60.0 kV/mm1520 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 50 Hz
0.0020
@Frequency 50 Hz
IEC 60250
 0.021
@Frequency 1e+6 Hz
0.021
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 35 V35 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 70.0 µm/m-°C38.9 µin/in-°FISO 11359
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°FIEC 1006
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FDIN 52 612
Melting Point 255 °C491 °FISO 11357
Maximum Service Temperature, Air 100 °C212 °Flong term
 180 °C356 °Fshort term
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FISO 75
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
LOI Acid Index (%)25ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Hippe PET Polyethylene Terephthalate
Overview of materials for PBT + PET Blend, Glass Filled
Overview of materials for Polycarbonate/PET Polyester Blend
Covestro Makroblend® UT305 PC/PET Blend

PPOLYPL926 / 197636

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.