MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength makes DA528 an excellent choice for profile extrusions, molding, and foaming applications requiring high VA content.

    Application/Uses
  • Flexible packaging films
  • Peelable seals, adhesive layers
  • Injection and blow molding
  • Hot melt adhesives and blends
  • Profile extrusions, tubing, wire & cable

Key Words: Excellent optics and low heat seal initiation. 18.5% EVA.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³D1505
Vinyl Acetate Content 18.5 %18.5 %
Thickness 38.1 microns1.50 milThickness Tested
Melt Flow 2.5 g/10 min2.5 g/10 minD1238
 
Mechanical PropertiesMetricEnglishComments
Dart Drop Test 10.2 g0.0225 lbD1709
 390 g0.860 lbD1709
Film Tensile Strength at Break, MD 24.8 MPa3600 psiD638
Film Tensile Strength at Break, TD 24.1 MPa3500 psiD638
1% Secant Modulus, MD 42.1 MPa6110 psiD882
1% Secant Modulus, TD 50.3 MPa7300 psiD882
 
Thermal PropertiesMetricEnglishComments
Melting Point 85.0 °C185 °FDSC Peak; D33418
 
Optical PropertiesMetricEnglishComments
Haze 3.5 %3.5 %D1003
Gloss 82 %82 %at 45; D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 °C379 °FBlown Film
 210 °C410 °FCast Film
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
processFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem PN2021 EVA Foam Copolymer
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer
Bamberger Polymers Bapolene® EVA-1120 Ethylene Vinyl Acetate (EVA)
Braskem Evateno® 3019 PE EVA Foam Copolymer
Braskem Evateno® 8019 PE EVA Foam Copolymer

PBP1129 / 133377

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.