MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Medalist® MD-17270 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-17270 is a high performance thermoplastic elastomer specifically designed for a peristaltic pump tubing applications. Medalist MD-17270 is a medium hardness, low density, sterilizable grade suitable for extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Abrasion Resistant; Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Colorability; Good Melt Strength; Halogen Free; Low Density; Medium Hardness; Radiation Sterilizable

Uses: Biopharma Processing. Hospital Goods; Medical Devices; Medical/Healthcare Applications; Pharmaceuticals; Rubber Replacement; Tubing

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 200 °C
15 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  70
@Time 5.00 sec
70
@Time 0.00139 hour
Injection Molded; ASTM D2240
 72
@Time 1.00 sec
72
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 12.1 MPa1750 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain  2.52 MPa
@Strain 100 %
365 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 3.59 MPa
@Strain 300 %
520 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 770 %770 %Die C, 20 in/min; ASTM D412
Tear Strength 40.3 kN/m230 pliDie C, 20 in/min; ASTM D624
Compression Set  24 %
@Temperature 22.8 °C,
Time 79200 sec
24 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395
 55 %
@Temperature 70.0 °C,
Time 79200 sec
55 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395
 
Processing PropertiesMetricEnglishComments
Zone 1 154 - 166 °C310 - 330 °F
Zone 2 166 - 182 °C330 - 360 °F
Zone 3 182 - 193 °C360 - 380 °F
Adapter Temperature 188 - 199 °C370 - 390 °F
Die Temperature 199 - 207 °C390 - 405 °F
Melt Temperature 188 - 199 °C370 - 390 °F
Screw Speed 30 - 100 rpm30 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-12362 Thermoplastic Elastomer
Teknor Apex Medalist® MD-12160H Thermoplastic Elastomer
Teknor Apex Medalist® MD-32265 Thermoplastic Elastomer
Teknor Apex Medalist® MD-50357 Thermoplastic Elastomer
Teknor Apex Medalist® MD-50263 Thermoplastic Elastomer

PTEKNQ0711 / 237202

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.