MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum AL 800H™ Nickel-Base Alloy, UNS N08810
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: AL 800H alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-corrosion cracking and to embrittlement form precipitation of sigma phase. The general corrosion resistance is excellent. This alloy has been approved as a material of construction under ASME Boiler and Pressure Vessel Code, Section I-Power Boilers, Section III-Nuclear Vessels, and Section VIII-Unfired Pressure Vessels. Uses include heat exchangers, process piping, heat treatment fixtures, furnace parts, and steam.

Information provided by Allegheny Ludlum

Key Words: DIN 1.4876; ASTM B-409; ASME SB-409; AMS 5871
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.08 g/cc0.292 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7070Typical Annealed
Tensile Strength, Ultimate 531 MPa77000 psiTypical; Annealed at 2100°F (1149°C)
Tensile Strength, Yield 200 MPa
@Strain 0.2 %
29000 psi
@Strain 0.2 %
Typical; Annealed at 2100°F (1149°C)
Elongation at Break 52 %52 %in 2"; Typical; Annealed at 2100°F (1149°C)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000990 ohm-cm0.0000990 ohm-cm
Magnetic Permeability <= 1.02<= 1.02
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.40 %0.40 %
Carbon, C 0.080 %0.080 %
Chromium, Cr 21 %21 %
Copper, Cu 0.30 %0.30 %
Iron, Fe 44 %44 %as balance
Manganese, Mn 1.0 %1.0 %
Nickel, Ni 32 %32 %
Phosphorus, P 0.020 %0.020 %
Silicon, Si 0.35 %0.35 %
Sulfur, S 0.010 %0.010 %
Titanium, Ti 0.40 %0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlson C 800H Nickel-Iron-Chromium Alloy
AISI 1006 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 (0.06-0.23 in) mm thick
ATI Allvac® Nickelvac® 800-H Nickel Superalloy (UNS N08810)
Special Metals INCOLOY® Alloy 800HT™
21Cr-32Ni-Ti-Al IRON BASED 21Cr-32Ni-Ti-Al ALLOY FOR HEAT EXCHANGER SEAMLESS TUBES (NCF 800H TB)

NLN80H / 18025

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.