MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 299 A X 117575 Nylon 6 (PA) Glass Fiber - Flame Retardant - Halogen Free
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: This product has been tested to have a Flame Spread Index of less than 25 per ASTM E-162 and a Smoke Developed Index of less than 200 at 4 mins in the flaming mode per ASTM E-662.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D 792
Additive Loading 30 %30 %Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 131 MPa19000 psiASTM D 638
Elongation at Break 4.0 %4.0 %ASTM D 638
Tensile Modulus 8.96 GPa1300 ksiASTM D 638
Flexural Strength 228 MPa33000 psiASTM D 790
Flexural Modulus 10.3 GPa1500 ksiASTM D 790
Izod Impact, Notched 1.23 J/cm
@Thickness 3.20 mm
2.30 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 10.7 J/cm
@Thickness 3.20 mm
20.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 199 °C390 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 213 °C415 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 243 - 279 °C470 - 535 °F
Mold Temperature 54.4 - 93.3 °C130 - 200 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.20 %0.20 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Descriptive Properties
Aerospace Ignition ResistanceF2FAR 25.853; 0.060 in. (1.5 mm)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
RTP Company RTP 299A X 68905 A  Nylon 6 (PA 6) Long Glass Fiber 40%
RTP Company RTP 205 A FR Nylon 6 (PA), Glass Fiber - Flame Retardant
RTP Company RTP 204 A FR UV Nylon 6 (PA), Glass Fiber - Flame Retardant - UV Stabilized
RTP Company RTP 204 A FR Nylon 6 (PA), Glass Fiber - Flame Retardant

PQZVA12347 / 120576

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.