MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 205 A FR Nylon 6 (PA), Glass Fiber - Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.65 g/cc1.65 g/ccASTM D 792
Water Absorption 1.2 %
@Time 86400 sec
1.2 %
@Time 24.0 hour
ASTM D 570
Additive Loading 30 %30 %Primary Additive
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0015 - 0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D 785
Tensile Strength at Break 155 MPa22500 psiASTM D 638
Elongation at Break 2.8 %2.8 %ASTM D 638
Tensile Modulus 12.4 GPa1800 ksiASTM D 638
Flexural Strength 241 MPa35000 psiASTM D 790
Flexural Modulus 10.3 GPa1500 ksiASTM D 790
Izod Impact, Notched 1.33 J/cm
@Thickness 3.20 mm
2.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 9.61 J/cm
@Thickness 3.20 mm
18.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D 257
Dielectric Constant 4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 18.7 kV/mm475 kV/inShort Term; In Oil; ASTM D 149
Dissipation Factor 0.013
@Frequency 1e+6 Hz
0.013
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C420 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 199 °C390 °FASTM D 648
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 243 - 279 °C470 - 535 °F
Mold Temperature 54.4 - 93.3 °C130 - 200 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.20 %0.20 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 25 F30 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
RTP Company RTP 203 A FR Nylon 6 (PA), Glass Fiber - Flame Retardant
Plastcom SLOVAMID 6 GF 5 FRA 5 Polyamide 6, 5% Glass Fiber, Halogen Flame Retardant
RTP Company RTP 201 A FR UV Nylon 6 (PA), Glass Fiber - Flame Retardant - UV Stabilized
RTP Company RTP 201 A FR Nylon 6 (PA), Glass Fiber - Flame Retardant

PQZWA1076 / 90542

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.