MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilon® BKZ-30 PA6-GB30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Bead Filled

Material Notes:

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³Dry; ISO 1183
Water Absorption 8.0 %8.0 %Sim. to ISO 62
Moisture Absorption 2.00 %2.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 85.0 MPa12300 psiConditioned; ISO 2039-1
 115 MPa16700 psiDry; ISO 2039-1
Tensile Strength at Break 40.0 MPa5800 psiConditioned; ISO 527-1/-2
 65.0 MPa9430 psiDry; ISO 527-1/-2
Elongation at Break 15 %15 %Dry; ISO 527-1/-2
 40 %40 %Conditioned; ISO 527-1/-2
Tensile Modulus 1.90 GPa276 ksiConditioned; ISO 527-1/-2
 3.40 GPa493 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveInterior
Electricals & ElectronicsElectrical appliances
FormGranules
Industry & Consumer goodsHousewares
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Special CharacteristicsHigh impact or impact modified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® BK-30 PA6-GB30
Omni Plastics OmniLon™ PA6 GB30 Nylon 6, 30% Glass reinforced
Eurotec® Tecomid® NB40 GB30 NL PA6, 30% glass bead reinforced, natural
Eurotec® Tecomid® NA40 GB30 NL HS PA6.6, 30% glass bead reinforced, heat stabilized, natural
EMS-Grivory Grilon® TSGK-30/4 X PA666-(GF+GB)30

PGRH200 / 156909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.