MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Premi-Glas® 3404 33% Glass Reinforced SMC
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required.

Key features and benefits:

  • Radiant panel flame spread index of less than 35 (ASTM E-162)
  • Smoke Density less than 25 (ASTM E-662)
  • In-mold powder color coating capable
  • Specially developed for low toxicity in rail and aircraft applications

Market: Mass Transit

Information provided by Premix.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.83 g/cc1.83 g/cc
Linear Mold Shrinkage 0.00030 cm/cm0.00030 in/inPolymerization Shrinkage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa13100 psiASTM D638
Tensile Modulus 10.0 GPa1450 ksiASTM D638
Flexural Strength 190 MPa27600 psiASTM D790
Flexural Modulus 10.0 GPa1450 ksiASTM D790
Poissons Ratio 0.300.30
Shear Modulus 3.80 GPa551 ksiCalculated
Izod Impact, Notched 5.50 J/cm10.3 ft-lb/inASTM D256
Izod Impact, Unnotched 9.50 J/cm17.8 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°FZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°C13.9 µin/in-°FXY Direction
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °FCompression Molding
Clamp Pressure 3.45 - 6.89 MPa500 - 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass
A. Schulman Premi-Glas® 1200-30 Polyester SMC
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP
A. Schulman Premi-Glas® 1200H-15 Polyester SMC

PPREMI35 / 58162

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.