MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Premi-Glas® 1200H-15 Polyester SMC
Categories: Polymer; Thermoset; Composite SMC; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame recognition is sufficient. Key features and benefits are:
  • Underwriters Laboratory UL 94HB flame recognition at 1.47mm minimum wall thickness.
  • U.L flame recognized in all colors.
  • Excellent flexural strength and flexural modulus properties.
  • Designed for compression molding in matched metal molds.
  • Available in fiberglass content of 10-30%.
  • The Premi-Glas 1200-H series carries U.L 746 C recognition for use in exterior applications following ultraviolet light, water emersion and exposure testing.

A. Schulman has acquired this former Premix product line.

Key Words: Sheet Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 - 1.85 g/cc1.70 - 1.85 g/cc
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm0.0015 - 0.0025 in/inPolymerization Shrinkage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.0 MPa5080 psiASTM D638
Tensile Modulus 12.0 GPa1740 ksiASTM D638
Flexural Strength 95.0 MPa13800 psiASTM D790
Flexural Modulus 9.50 GPa1380 ksiASTM D790
Compressive Strength 145 MPa21000 psiASTM D695
Poissons Ratio 0.300.30
Shear Modulus 4.60 GPa667 ksiCalculated
Izod Impact, Notched 4.25 J/cm7.96 ft-lb/inASTM D256
Izod Impact, Unnotched 6.00 J/cm11.2 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 15.0 kV/mm381 kV/inASTM D149
Arc Resistance 180 sec180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°FZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°C13.9 µin/in-°FXY Direction
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
UL RTI, Electrical 130 °C266 °FUL 746C
UL RTI, Mechanical with Impact 130 °C266 °FUL 746C
UL RTI, Mechanical without Impact 130 °C266 °FUL 746C
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °FCompression Molding
Clamp Pressure 3.45 - 6.89 MPa500 - 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1200-30 Polyester SMC
A. Schulman Premi-Glas® 1200H-20 Polyester SMC
A. Schulman Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC
A. Schulman Premi-Glas® 1203-30 Fiberglass Reinforced SMC
A. Schulman Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC

PPREMIX08 / 58173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.