MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Moplen HP520H Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Moplen HP520H is a polypropylene homopolymer especially designed for the production of biaxial oriented polypropylene films (BOPP). It contains a general purpose formulation. Typical applications of Moplen HP520H are film for adhesive tapes and general packaging. Applications: Food Packaging Film, Raffia/Tapes/Strapping.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7171ISO 868
Tensile Strength at Break 23.0 MPa3340 psi50mm/min; ISO 527-1,-2
Tensile Strength, Yield 34.0 MPa4930 psi50mm/min; ISO 527-1,-2
Elongation at Break >= 500 %>= 500 %50mm/min; ISO 527-1,-2
Elongation at Yield 12 %12 %50mm/min; ISO 527-1,-2
Flexural Modulus 1.45 GPa210 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 155 °C311 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 0.30 %0.30 %ASTM D1003
 
Descriptive Properties
Processing MethodBOPP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Adstif HA 3105 Polypropylene
Dow DX5E66 Polypropylene Homopolymer Resin
Borealis Bormed™ RB801CF Polypropylene Random Copolymer
LyondellBasell Moplen RP2795 Polypropylene Copolymer
LyondellBasell Moplen HP522H Polypropylene

PEQT9029 / 220660

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.