Moplen HP520H is a polypropylene homopolymer especially designed for the production of biaxial oriented polypropylene films (BOPP). It contains a general purpose formulation. Typical applications of Moplen HP520H are film for adhesive tapes and general packaging. Applications: Food Packaging Film, Raffia/Tapes/Strapping.Information provided by LyondellBasell. |