MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Armacell Ensolite™ IV1 PVC/NBR/CR
Categories: Polymer; Thermoplastic; Vinyl (PVC); Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Armacell LLC (Conover, NC Plant) manufactures a black, continuous, (rolls / sheets) closed cell, 3.0 - 5.5 lb/ft3 (48 - 88 kg/ m3) density, PVC/ NBR / CR rubber product IV1, that meets all the physical property requirements of ASTM D 1056-14 2A1 / 2C1.
  • Has good resistance to oil & fuel.
  • Manufactured with nonstaining oils and anti-oxidants.
  • Meets the horizontal burn / flame requirements of FMVSS-302 at most thicknesses.
  • Listed to UL94 HF-1 at 1.3 mm (0.051") and UL94 V-0 at 11.7 mm (0.460") and higher (UL File # QMFZ2.E55798).
  • Listed with UL to UL50E [periodic & continuous compression] (UL File # JMST2. MH10189).
  • Listed on the approved source list for Chrysler MSAY 516 Type 1.

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0481 - 0.0881 g/cc0.00174 - 0.00318 lb/in³ASTM D1056
Water Absorption <= 10 %<= 10 %ASTM D1056
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 30 - 5030 - 50ASTM D2240
Tensile Strength >= 0.345 MPa>= 50.0 psiASTM D412, Die A
Elongation at Break >= 100 %>= 100 %ASTM D412, Die A
Compressive Strength 0.0138 - 0.0345 MPa
@Strain 25 %
2.00 - 5.00 psi
@Strain 25 %
ASTM D1056
Tear Strength >= 1.58 kN/m>= 9.00 pliDie C; ASTM D624
Compression Set <= 40 %
@Strain 50 %
<= 40 %
@Strain 50 %
ASTM D1056
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.3 °C200 °FIntermittent; ASTM D1056
Minimum Service Temperature, Air -40.0 °C-40.0 °FASTM D1056
Flammability, UL94  V-1
@Thickness 11.7 mm
V-1
@Thickness 0.461 in
 V-0
@Thickness 11.7 mm
V-0
@Thickness 0.461 in
 
Descriptive Properties
Accelerated Aging±30%Change in Compression Deflection, 7 days at 70°C, ASTM D1056
FlammabilityFMVSS302Pass @ most thicknesses
 HF-1>1.3 mm
Fluid Immersion<250%Weight Change, 7 days at 23°C, Fuel B, ASTM D1056

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell Ensolite™ GIC Continuous Rolls/Sheets, PVC/NBR
Armacell Ensolite™ IV2 PVC/NBR/CR
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Armacell Ensolite™ IG1 PVC/NBR/CR
Armacell Ensolite™ IFC-400 Continuous Rolls/Sheets, PVC/NBR

PARMD073 / 186684

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.