MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Impact Polystyrene 940E Super High Impact Polystyrene, Sheet Extrusion and Thermoforming Grade
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: TOTAL Petrochemicals 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.

Applications: The combination of high gloss, toughness and high stiffness makes 940E an excellent choice for cups, food packaging, custom sheet and coextrusion applications. An excellent high gloss resin for specialty injection appliance and electronic applications.

General Information:

  • This material complies with FDA requirements as described in 21 CFR § 177.1640.
  • This material holds Underwriters Laboratory recognition 94HB; see UL file E55470.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/cc
Water Absorption <= 0.10 %<= 0.10 %
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 2.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.8 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.2 MPa3800 psiASTM D638
Elongation at Yield 50 %50 %ASTM D638
Tensile Modulus 2.07 GPa300 ksiASTM D638
Flexural Strength 47.6 MPa6900 psiASTM D790
Flexural Modulus 2.07 GPa300 ksiASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
Impact Test 217 J
@Thickness 25.4 mm
160 ft-lb
@Thickness 1.00 in
Falling Dart; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 101 °C214 °FASTM D1525
Heat Distortion Temperature 93.9 °C201 °FAnnealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss 92 %92 %60°; ASTM D523
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PSC 1540(AS) Crystal Polystyrene
Supreme Petrochem SC 208 General Purpose Polystyrene
Total PSI 940E Impact Polystyrene
Total PSI 7240 High Impact Polystyrene
Resirene Resirene® HF-777 General Purpose Polystyrene

PTOTAL891 / 130616

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.