WACKER® E 32 is a nonionic, aqueous emulsion of a silicone wax which is solid at room temperature. WACKER® E 32 can be readily incorporated into cold stirred formulations. Application: WACKER® E 32 is mainly used in the polishes sector. The affinity of the active ingredient to various substrates confers the aqueous formulations with outstanding resistance to detergents and weathering. Information provided by Wacker Chemie AG. |