MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Wacker® E 32 Silicone Wax Emulsion
Categories: Polymer; Thermoset; Silicone

Material Notes: WACKER® E 32 is a nonionic, aqueous emulsion of a silicone wax which is solid at room temperature. WACKER® E 32 can be readily incorporated into cold stirred formulations.

Application: WACKER® E 32 is mainly used in the polishes sector. The affinity of the active ingredient to various substrates confers the aqueous formulations with outstanding resistance to detergents and weathering.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 40 %
Particle Size 190 µm
pH 5.0
 
Descriptive Properties
Appearancemilky

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3003/30 A/B Liquid Silicone Rubber
Overview of materials for Silicone Elastomer, for Thermal Management
Wacker Wacker® E 22 Silicone Fluid Emulsion
Wacker Elastosil® LR 3003/50 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3003/20 TR A/B Liquid Silicone Rubber

PWACK9746 / 205275

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.