MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Iran Petrochemical (PCC) SBR-1502 Styrene Butadiene Rubber
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: SBR–1502 is a cold, 23.5% styrene SBR polymer made with a mixed-acid emulsifier, a non-staining stabilizer and a salt–acid coagulation. Provided that the compounds are formulated and processed correctly, the vulcanizates have very good abrasion , good heat and aging resistance, good mechanical properties , good electrical properties and good resistance to polar solvents and dilute acids.

Applications: end uses include white sidewall tyres, foot wear, light and dark coloured mechanical goods and miscellaneous items where excellent physical properties and minimum discoloration and staining are required.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %ASTM D1416
Viscosity Measurement 46 - 5846 - 58raw viscosity, ML 1+4 @ 100°C; ASTM D1646
Mooney Viscosity <= 84<= 84compound viscosity, ML 1+4 @ 100°C; ASTM D1646
Ash <= 1.5 %<= 1.5 %ASTM D1416
 
Chemical PropertiesMetricEnglishComments
Styrene Content 23 %23 %ASTM D1416
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 24.5 MPa>= 3560 psi35 min cured; ASTM D412
Elongation at Break 350 %350 %35 min cured; ASTM D412
300% Modulus 16.4 - 20.3 MPa
@Strain 300 %
2380 - 2940 psi
@Strain 300 %
35 min cured; ASTM D412
 
Descriptive Properties
Organic Acid, %5.875ASTM D1416
Soap, %< 0.5ASTM D1416

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) SBR-1500 Styrene Butadiene Rubber
Iran Petrochemical (PCC) SBR-1712 Styrene Butadiene Rubber
LG Chemical SBR 1502 High Acrylonitrile Polymer
Iran Petrochemical (PCC) PVC-S6058 Poly Vinyl Chloride
Iran Petrochemical (PCC) PVC-S6558 Poly Vinyl Chloride

PIPC359 / 149793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.