Iran Petrochemical (PCC) PVC-S6558 Poly Vinyl Chloride
Categories:
Polymer
;
Thermoplastic
;
Vinyl (PVC)
;
PVC, Flexible Grade
Material Notes:
Grade S6558 has low porosity & high bulk density.
Applications: pipe and fitting, injection molding
Information provided by Iran Petrochemical Commercial Co.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.600
g/cc
0.0217
lb/in³
DIN-53466
Volatiles
<= 0.20 %
<= 0.20 %
weight %; ISO R-1269
Viscosity Test
105
cm³/g
1.05
dl/g
DIN-53726
Ash
<= 0.050 %
<= 0.050 %
Sulfate ash, weight %; DIN-53568/2
Component Elements Properties
Metric
English
Comments
Chlorine, Cl
56 %
56 %
by weight
Descriptive Properties
Dark Resin, particles
30
per 250 g PVC; HULS-6.9
K-Value
65
DIN-53726
Residual Vinyl Chloride Monomer, ppm
=1
HULS-6.11
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Iran Petrochemical (PCC) PC 1218 Polycarbonate
Iran Petrochemical (PCC) SBR-1500 Styrene Butadiene Rubber
Iran Petrochemical (PCC) PVC-S6058 Poly Vinyl Chloride
Iran Petrochemical (PCC) PVC-S7054 Poly Vinyl Chloride
Iran Petrochemical (PCC) HB0035 High Density Polyethylene
PIPC325 / 149759
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.