MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lehvoss LUVOCOM® 3/CF/30 VP Polyamide 6 with carbon fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Properties/attributes include: Very strong and stiff parts; low coefficient of thermal expansion. Dynamic-stress and wear-resistant parts. Electrically conductive, suitable for continuous discharging of statically-generated electricity.

Automotive industry, textile machinery, apparatus- and precision engineering. Typical uses include: Handles, levers, rollers, extrusion profiles.

Processing: During processing the moisture level should not exceed 0.1%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Excessively high predrying temperatures may cause discoloration. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/ccISO 1183
Moisture Absorption <= 1.00 %
@Temperature 23.0 °C,
Time 86400 sec
<= 1.00 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 220 MPa31900 psiISO 527-2
Elongation at Break 2.2 %2.2 %ISO 527-2
Modulus of Elasticity 21.0 GPa3050 ksiISO 527-2
Flexural Strength 330 MPa47900 psiISO 178
Flexural Modulus 19.0 GPa2760 ksiISO 178
Flexural Strain at Break 2.8 %2.8 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1fu
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 1000 ohm-cm<= 1000 ohm-cmIEC 60167
Surface Resistance <= 1000 ohm<= 1000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C11.1 µin/in-°FDIN 53752
Thermal Conductivity 0.500 W/m-K3.47 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 90.0 °C194 °FContinuous; UL 746B
 210 °C410 °FShort Term
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 270 - 280 °C518 - 536 °F
Zone 1 250 - 270 °C482 - 518 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 270 °C518 °F
Mold Temperature 70.0 - 110 °C158 - 230 °F
Drying Temperature  75.0 °C
@Time 36000 - 57600 sec
167 °F
@Time 10.0 - 16.0 hour
Dehumidifying dryer
 105 °C
@Time 14400 - 21600 sec
221 °F
@Time 4.00 - 6.00 hour
Dehumidifying dryer
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Colornatural color (black)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CP-Polymer-Technik Wellamid® 6000 CF 30 HWCP 30% Carbon Fiber Nylon 6, Heat Stabilized, Dry
CP-Polymer-Technik Wellamid® 6000 CF 30 HWCP 30% Carbon Fiber Nylon 6, Heat Stabilized, Conditioned
BASF Ultradur® B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET

PLUU8913 / 193872

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.