MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Styrolux® 3G55 SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrolux® 3G55 is a clear styrene butadiene copolymer (SBC) used mainly in sheet extrusion and thermoforming applications. It is specifically designed for improved performance in blends with general-purpose polystyrene, providing parts with an excellent balance of toughness, transparency and economics. Because of the tendency of blocking, 3G55 is mainly used in inline thermoforming. 3G55 is difficult to print and decorate since it contains a microcrystalline wax. Outstanding toughness, highest GPPS blend capacity, good clarity. Applications: Food and non-food packaging, Food service items, Drinking cups, Extruded films, In-line thermoforming.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Water Absorption at Saturation 0.070 %
@Temperature 23.0 °C
0.070 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0030 - 0.010 cm/cm0.0030 - 0.010 in/inISO 294-4
Melt Flow 14 g/10 min
@Load 5.00 kg,
Temperature 200 °C
14 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858ISO 868
Tensile Strength, Yield 15.0 MPa2180 psiISO 527
Elongation at Break >= 300 %>= 300 %Nominal; ISO 527
 >= 300 %>= 300 %ISO 527
Elongation at Yield 2.0 %2.0 %ISO 527
Tensile Modulus 0.900 GPa131 ksiISO 527
Flexural Strength 18.0 MPa2610 psiISO 178
Flexural Yield Strength 18.0 MPa
@Strain 5.0 %
2610 psi
@Strain 5.0 %
Flexural Modulus 0.900 GPa131 ksiISO 178
Izod Impact, Notched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Instrumented Impact Energy at Peak 10.0 J7.38 ft-lbInstrumented Dart Impact (Energy at Peak Force); ASTM Test
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.00030
@Frequency 100 Hz
0.00030
@Frequency 100 Hz
IEC 60250
 0.00080
@Frequency 1e+6 Hz
0.00080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 90.0 µm/m-°C33.3 - 50.0 µin/in-°FISO 11359
CTE, linear, Transverse to Flow 72.0 µm/m-°C40.0 µin/in-°FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C144 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C124 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  35.0 °C
@Load 5.10 kg
95.0 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 67.0 °C
@Load 1.02 kg
153 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.571.57Sodium D Line; ISO 489
Haze 3.0 %3.0 %ASTM D1003
Transmission, Visible 89 %
@Wavelength 550 nm
89 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °FISO 294
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF NoNoNSF Std. 51
 NoNoNSF Std. 61
 
Descriptive Properties
ColorClear
Commercial StatusActive America
FormYes
Impact ModifiedYes
Primary Processing TechniqueExtrusion
ProcessingBlow Molding
 Film Extrusion
 Injection Molding
 Other Extrusion
 Sheet Extrusion
UL.UL-CNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Styrolux® 3G33 SBC
ExxonMobil LLDPE LL 8446.21 Linear Low Density Polyethylene Resin (European Grade)
INEOS Styrolution Luran® S KR 2859 ASA
INEOS Styrolution Luran® S Q440 ASA
Overview of materials for High Density Polyethylene (HDPE), Extruded

PBASF9029 / 84793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.