MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Luran® S KR 2859 ASA
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: Luran® S KR 2859, a stiff extrusion product. Versatile grade for profile and sheet extrusion as protective cap layer. high stiffness, high impact strength. Applications: profile extrusion, sheet extrusion, protective cap layer.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Melt Flow 12 g/10 min
@Load 10.0 kg,
Temperature 220 °C
12 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psiISO 527
Elongation at Break 7.0 %7.0 %ISO 527
Elongation at Yield 3.6 %3.6 %ISO 527
Tensile Modulus 2.50 GPa363 ksiISO 527
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 16.0 J/cm²
@Temperature 23.0 °C
76.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 1200 MPa174000 psiISO 899
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 110 µm/m-°C44.4 - 61.1 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Vicat Softening Point 98.0 °C
@Load 5.10 kg
208 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 230 °C410 - 446 °FISO 294
Mold Temperature 60.0 °C140 °FISO 294
 
Descriptive Properties
ColorNatural
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® S 778T ASA
INEOS Styrolution Luran® S 797S White 35962 ASA
Ineos ABS Centrex® 814 ASA Blend
Ineos ABS Centrex® 815 ASA Blend
Ineos ABS Centrex® 821 ASA Blend

PBASG0586 / 132219

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.