MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lord Adhesives Thermoset™ MT-125 Thermally Conductive Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Thermoset™ MT-125 thermally conductive adhesive is a rapid cure, one-component adhesive specifically designed for applications requiring a long working life adhesive with high thermal conductivity. Thermoset MT-125 adhesive is suitable for use as a thermal interface adhesive for heat sink attachment and other applications requiring good adhesion and heat transfer properties.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.10 g/cc2.10 g/cc
Viscosity 95000 - 115000 cP
@Temperature 25.0 °C
95000 - 115000 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Modulus of Elasticity 7.00 GPa
@Temperature 30.0 °C
1020 ksi
@Temperature 86.0 °F
Storage
Shear Strength 20.68 MPa
@Temperature 2998.6 °C
2999 psi
@Temperature 5429.5 °F
AL/AL
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+13 ohm-cm
@Temperature 25.0 °C
2.00e+13 ohm-cm
@Temperature 77.0 °F
ASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 31.0 µm/m-°C17.2 µin/in-°FAlpha 1
 73.0 µm/m-°C40.6 µin/in-°FAlpha 2
Thermal Conductivity 2.35 W/m-K16.3 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 123 °C253 °FTMA
 
Processing PropertiesMetricEnglishComments
Cure Time  8.00 min
@Temperature 150 °C
0.133 hour
@Temperature 302 °F
 30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
Pot Life 20160 min
@Temperature 25.0 °C
20160 min
@Temperature 77.0 °F
Shelf Life 6.00 Month
@Temperature -30.0 °C
6.00 Month
@Temperature -22.0 °F
 
Descriptive Properties
AppearanceGray
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives 8651 Polymer Resistor Composition
Lord Adhesives Thermoset™ ME-531 Underfill Encapsulant
Lord Adhesives Thermoset™ TC-228 Thermally Conductive Grease
Lord Adhesives Thermoset™ MD-200 Electrically Conductive Die-Attach Adhesive
Epoxy Technology EPO-TEK® T905BN-3 Thermally Conductive Epoxy

PLORD034 / 86042

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.