MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Bentolite® 2422 Calcium Bentonite
Categories: Ceramic; Clay

Material Notes: Bentolite 2422 is a specially processed calcium bentonite which is suited for coating applications where control of settling and syneresis are needed. Bentolite 2422 is a high brightness bentonite clay. Bentolite 2422 will also improve hiding. Bentolite 2422 improves hold-out, particularly when used in conjunction with cellulosics. Improved hold-out is useful when painting over a porous substrate, painting a substrate with different densities (i.e. gypsum wall board with joint compound), and touchup of a previously painted surface.

Uses and Advantages:

  • Controls Settling
  • Controls Syneresis
  • Improves Hiding
  • Improves Hold-out
  • Excellent Wet Edge Properties

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.481 g/cc0.0174 lb/in³loose
 0.721 g/cc0.0260 lb/in³packed
Brightness 60 %60 %
Particle Mesh Size 200 Mesh200 Mesh95%
pH 9.59.52% Slurry
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 8.0 %8.0 %
Iron, Fe 0.60 %0.60 %Soluble
 
Descriptive Properties
Color/FormOff White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Bentolite® 865 Texas Bentonite
BYK Bentolite® C Bentonite
BYK Bentolite® BK Bentonite
BYK Bentolite® H Bentonite
BYK Advitrol® 8-10 Rheological additive

PBYK006 / 185003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.