System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
INEOS Styrolution Luran® 368R SAN
Categories:
Polymer
;
Thermoplastic
;
SAN Polymer
;
Styrene Acrylonitrile (SAN), Molded
Material Notes:
General-purpose grade with well-balanced properties intended for both injection molding and extrusion.
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Key Words:
368 R
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.08
g/cc
0.0390
lb/in³
ISO 1183
Linear Mold Shrinkage
0.0050
cm/cm
0.0050
in/in
ASTM Data; MD
Melt Flow
10
g/10 min
@Load 10.0 kg,
Temperature 220 °C
10
g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
104
MPa
@Temperature -40.0 °C
15100
psi
@Temperature -40.0 °F
ISO Data
Tensile Strength, Ultimate
75.0
MPa
10900
psi
5mm/min; ISO 527
Tensile Strength, Yield
75.0
MPa
10900
psi
2 in/min; ASTM Test
32.0
MPa
@Temperature 80.0 °C
4640
psi
@Temperature 176 °F
ISO Data
Elongation at Break
3.0 %
3.0 %
5mm/min; ISO 527
3.0 %
3.0 %
2 in/min; ASTM Test
3.7 %
@Temperature -40.0 °C
3.7 %
@Temperature -40.0 °F
ISO Data
Elongation at Yield
2.1 %
@Temperature 80.0 °C
2.1 %
@Temperature 176 °F
ISO Data
Tensile Modulus
3.70
GPa
537
ksi
1mm/min; ISO 527
3.80
GPa
551
ksi
ASTM Test
Flexural Strength
125
MPa
18100
psi
ASTM Test
Charpy Impact Unnotched
1.80
J/cm²
8.57
ft-lb/in²
ISO 179
1.80
J/cm²
@Temperature -30.0 °C
8.57
ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched
0.200
J/cm²
0.952
ft-lb/in²
ISO 179
Tensile Creep Modulus, 1 hour
3500
MPa
508000
psi
ISO 899
Tensile Creep Modulus, 1000 hours
2800
MPa
406000
psi
ISO 899
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+13
ohm-cm
>=
1.00e+13
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+13
ohm
>=
1.00e+13
ohm
IEC 60093
Dielectric Constant
2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
IEC 60250
3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength
34.0
kV/mm
864
kV/in
IEC 60243-1
Dissipation Factor
0.0040
@Frequency 100 Hz
0.0040
@Frequency 100 Hz
IEC 60250
0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
425
V
425
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
70.0
µm/m-°C
38.9
µin/in-°F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi)
102
°C
216
°F
annealed; ASTM Test
102
°C
216
°F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
98.0
°C
208
°F
annealed; ASTM Test
98.0
°C
208
°F
ISO 75
Vicat Softening Point
106
°C
223
°F
Rate "A" Loading 1 (50 degC/h 10N); ASTM Test
106
°C
223
°F
(50 °C/h / 50N) - B/50; ISO 306
Oxygen Index
18 %
18 %
ISO 4589-1/-2
Optical Properties
Metric
English
Comments
Transmission, Visible
80 %
80 %
unknown thickness
Processing Properties
Metric
English
Comments
Melt Temperature
250
°C
482
°F
Injection molding
Mold Temperature
60.0
°C
140
°F
Injection molding
98.0
°C
208
°F
Ejection temperature
Injection Velocity
200
mm/sec
7.87
in/sec
Injection molding
Compliance Properties
Metric
English
Comments
FDA
Yes
Yes
NSF
No
No
NSF Std. 51
No
No
NSF Std. 61
Descriptive Properties
Color
Clear
Commercial Status
North America and Europe
Form
Pellets
Impact Modified
No
Primary Processing Technique
Extrusion
Processing
Injection Molding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Thermoforming
UL.UL-C
Yes
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
INEOS Styrolution Luran® SAN 51 Styrene Acrylonitrile
INEOS Styrolution Luran® SAN C Styrene Acrylonitrile
LG Chemical HI121H ABS, High Stiffness
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
INEOS Styrolution Luran® HD-20 SAN
PBASF9002 / 84766
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.