MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Luran® SAN C Styrene Acrylonitrile
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: Luran SAN C is an injection molding grade of SAN with medium impact strength and high flow.

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 23 g/10 min
@Load 10.0 kg,
Temperature 220 °C
23 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 68.0 MPa9860 psiISO 527
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 104 °C
@Load 5.10 kg
219 °F
@Load 11.2 lb
120°C/h; ASTM D 1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® SAN 51 Styrene Acrylonitrile
INEOS Styrolution Luran® 368R SAN
INEOS Styrolution Absolan® 2150 SAN
Chi Mei Kibisan® PN-127 SAN
INEOS Styrolution Absolan® 2300 SAN

PBASF8024 / 159706

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.