MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® NBX-0025 NF2001 PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Ultramid NBX-0025 NF2001 is a specialty, unfilled PA6/6.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³dry; ISO 1183
Water Absorption 8.5 %8.5 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.5 %2.5 %beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 54.0 MPa7830 psi50mm/min; ISO 527
Elongation at Break >= 50 %>= 50 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 25 %25 %50mm/min; ISO 527
Tensile Modulus 1.20 GPa174 ksi1mm/min; ISO 527
Flexural Modulus 1.10 GPa160 ksiISO Data
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO Test
Charpy Impact Unnotched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.60 J/cm²7.61 ft-lb/in²ISO 179
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 257 °C495 °F10 K/min
 257 °C495 °FASTM Test
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 1003-2 NF2002 PA66 (Conditioned)
Epsan Eplamid 66 IMP NC Q1C201 Polyamide 66
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Conditioned
Envalior Durethan® DP 2325 H3.0 000000 Nylon 66 (PA66), Conditioned
Envalior Durethan® A 30 S 000000 Nylon 6 (PA6), Conditioned

PBASF9382 / 85146

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.