System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Conditioned
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Unreinforced
Material Notes:
PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.143
g/cc
0.04129
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.0114
cm/cm
0.0114
in/in
60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0122
cm/cm
0.0122
in/in
60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Mechanical Properties
Metric
English
Comments
Puncture Resistance
2396
N
@Temperature 23.0 °C
538.6
lb (f)
@Temperature 73.4 °F
ISO 6603-2
Ball Indentation Hardness
70.0
MPa
10200
psi
ISO 2093-1
Tensile Strength at Break
55.0
MPa
7980
psi
5 mm/min; ISO 527-1,-2
Tensile Strength, Yield
55.0
MPa
7980
psi
50 mm/min; ISO 527-1,-2
Elongation at Break
155 %
155 %
Nominal, 50 mm/min; ISO 527-1,-2
230 %
230 %
5 mm/min; ISO 527-1,-2
Elongation at Yield
20 %
20 %
50 mm/min; ISO 527-1,-2
Tensile Modulus
1.40
GPa
203
ksi
1 mm/min; ISO 527-1,-2
Flexural Strength
49.0
MPa
7110
psi
2 mm/min; ISO 178-A
Flexural Yield Strength
36.0
MPa
@Strain 3.5 %
5220
psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
1.30
GPa
189
ksi
2 mm/min; ISO 178-A
Flexural Strain at Break
8.0 %
8.0 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
10.0
kJ/m²
@Temperature 23.0 °C
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)
130
kJ/m²
@Temperature -30.0 °C
61.9
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched
18.5
J/cm²
@Temperature -30.0 °C
88.0
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched
<=
1.00
J/cm²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
1.50
J/cm²
@Temperature 23.0 °C
7.14
ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Puncture Energy
27.2
J
@Temperature 23.0 °C
20.1
ft-lb
@Temperature 73.4 °F
ISO 6603-2
Thermal Properties
Metric
English
Comments
Melting Point
265
°C
509
°F
10°C/min; ISO 11357-1,-3
Processing Properties
Metric
English
Comments
Melt Temperature
260
°C
500
°F
injection molding
260
-
270
°C
500
-
518
°F
Mold Temperature
80.0
°C
176
°F
injection molding
80.0
-
100
°C
176
-
212
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultramid® 1003-2 NF2002 PA66 (Conditioned)
Plastcom SLOVAMID 66 HI/1 PA66, improved strength
Epsan Eplamid 66 IMP NC Q1C201 Polyamide 66
Envalior Durethan® DP 2325 H3.0 000000 Nylon 66 (PA66), Conditioned
Envalior Durethan® A 30 S 000000 Nylon 6 (PA6), Conditioned
PLANW9481 / 208336
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.