MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 1017 Steel, cold drawn
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Medium-low carbon steels have good weldability and slightly better machinability than the lower carbon steels. Relatively soft and strengthen with cold work during forming or drawing

Key Words: AFNOR NF A35-556 XC18, AIR 9160-C21 9160C011, DIN 17210 1.1141, DIN 17210 Ck15, MSZ 500 B38 X (Hungary), AFNOR XC15, AFNOR NF A35-551 XC18, AFNOR NF A35-552 XC18, AFNOR NF A35-553 XC18S, AFNOR NF A35-554 XC18S, carbon steels, UNS G10170, ASTM A29 1017, ASTM A29 M1017, ASTM A510 1017, ASTM A513 1017, ASTM A519 1017, ASTM A575 M1017, ASTM A635 1017, ASTM A659 1017, ASTM A830 1017, MIL-S-11410 1017, MIL S-11410 CS1017, BDS 2592 BSt3kp (Bulgaria), BDS 2592 BSt3ps, BDS 2592 BSt3sp, BDS 9801 VSt3kp, BDS 9801 VSt3ps, BDS 9801 VSt3sp, BDS 9801 WSt3kp, BDS 9801 WSt3ps, BDS 9801 WSt3sp, GB 714 A3q (China), GB 900 B3, GB 900 B3F, GB 900 C3, GB 300 C3F, JIS S15C, JIS S15CK, JIS G4051 S17C, DGN B-301 1017 (Mexico), COPANT 333 1017, STAS 10607 16 (Romania), PN 84023 18A (Poland), PN 84023 St3NO, PN 84024 R45, PN 84024 R45A, PN 84024 St44K, SAE J1397 1017, SAE J403 1017, SAE J412 1017, ONORM M3110 RC15 (Australia), NBN 253-03 C16-2 (Belgium), AISI1017
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 116116
Hardness, Knoop 135135Converted from Brinell
Hardness, Rockwell B 6666Converted from Brinell
Hardness, Vickers 120120Converted from Brinell
Tensile Strength, Ultimate 405 MPa58700 psi
Tensile Strength, Yield 340 MPa49300 psi
Elongation at Break 18 %18 %In 50 mm
Reduction of Area 40 %40 %
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Machinability 65 %65 %Based on AISI 1212 steel = 100%
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000159 ohm-cm
@Temperature 0.000 °C
0.0000159 ohm-cm
@Temperature 32.0 °F
estimated by comparison with similar materials
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.481 J/g-°C
@Temperature >=95.0 °C
0.115 BTU/lb-°F
@Temperature >=203 °F
condition unknown
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°Festimated based on similar materials
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.14 - 0.20 %0.14 - 0.20 %
Iron, Fe 99.11 - 99.56 %99.11 - 99.56 %As remainder
Manganese, Mn 0.30 - 0.60 %0.30 - 0.60 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1018 Steel, cold drawn
AISI 1016 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1020 Steel, normalized at 925°C (1700°F), air cooled, 25 mm (1 in.) round
AISI 1017 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1006 Steel, cold drawn

M1017A / 6807

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.