MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe LSS™ 2714T Hot Work Tool Steel (DIN 1.2714 mod)
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Hot Work Steel

Material Notes: TLS 2714HT is the same steel available from inventory in a heat-treated condition, at a hardness of 352 to 401 HBS (approximately 38 to 43 HRC). TLS 2714HT can be readily flame cut, and this property is often used to advantage in manufacturing hot extrusion die backer plates. TLS 2714HT should be considered for applications which require higher tensile strengths than the common pre-hardened steels such as 4140 and 4340.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.78 g/cc0.281 lb/in³Value supplied by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5353Air Cooled from 860°C, 45 minutes
 5555Oil Quenched from 830°C, 45 minutes
 5757Air Cooled from 900°C, 45 minutes
 5959Oil Quenched from 870°C, 45 minutes
Machinability 75 - 80 %75 - 80 %1% Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.2 µm/m-°C
@Temperature 20.0 - 100 °C
6.78 µin/in-°F
@Temperature 68.0 - 212 °F
 14.2 µm/m-°C
@Temperature 20.0 - 500 °C
7.89 µin/in-°F
@Temperature 68.0 - 932 °F
Thermal Conductivity  35.0 W/m-K
@Temperature 700 °C
243 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 36.0 W/m-K
@Temperature 20.0 °C
250 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 38.0 W/m-K
@Temperature 350 °C
264 BTU-in/hr-ft²-°F
@Temperature 662 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 732 °C1350 °FCritical Temperaure Ac1
 771 °C1420 °FCritical Temperaure Ac3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.50 %0.50 %
Chromium, Cr 1.3 %1.3 %
Iron, Fe 94.85 %94.85 %
Manganese, Mn 0.85 %0.85 %
Molybdenum, Mo 0.50 %0.50 %
Nickel, Ni 1.65 %1.65 %
Silicon, Si 0.25 %0.25 %
Vanadium, V 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe LSS™ 2714 Hot Work Tool Steel (DIN 1.2714 mod)
AISI Type L6 Low Alloy Tool Steel (UNS T61206)
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel
Latrobe LSS™ L6 Tool Steel (ASTM L6)
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel

NTIMK097 / 19444

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.