MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro DESMOPHEN® C 2100 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Linear, hydroxyl-terminated, aliphatic polycarbonate diol with a molecular weight of approx. 1,000 g/mol. High-grade building block for a variety of polyurethane systems.

Properties / Applications: In combination with polyisocyanates as a high-grade building block for the formulation of polyurethane systems with very good weatherability, lightfastness and hydrolytic stability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccDIN 51757
Viscosity 300 - 520 cP300 - 520 cPM014-ISO 3219/A.3
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.100.10[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesMetricEnglishComments
Solidus 33.0 - 62.0 °C91.4 - 144 °FISO 3016
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.050 %0.050 %DIN 51 777/1
 
Descriptive Properties
Color<150Hazen, M017-EN 1557
Content3.0-3.6%Hydroxyl, M023-DIN 53240-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMOPHEN® 651 MPA Polyurethane
Covestro DESMOPHEN® 650A-65 PMA Polyurethane
Covestro DESMOPHEN® 650 MPA Polyurethane
Covestro DESMOPHEN® 631 MPA Polyurethane
Covestro DESMOPHEN® C 1200 Polyurethane

PCOVEST0744 / 202527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.