MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Starex® BF-0677HF MABS, Unreinforced Scratch Resistant
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifier

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 3.20 mm
0.0040 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 3.20 mm
0.0050 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 19 g/10 min
@Load 10.0 kg,
Temperature 220 °C
19 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ASTM D785
Tensile Strength at Break 29.4 MPa4260 psi5 mm/min; ASTM D638
Tensile Strength, Yield 47.1 MPa6830 psi5 mm/min; ASTM D638
Elongation at Break 15 %15 %5 mm/min; ASTM D638
Tensile Modulus 2.39 GPa347 ksi5 mm/min; ASTM D638
Flexural Strength 68.6 MPa9950 psi2.8 mm/min; ASTM D790
Flexural Modulus 2.45 GPa356 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched  0.883 J/cm
@Thickness 6.35 mm
1.65 ft-lb/in
@Thickness 0.250 in
ASTM D256
 1.18 J/cm
@Thickness 3.17 mm
2.20 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
@Thickness 6.40 mm
199 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
@Thickness 6.40 mm
183 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 96.0 °C205 °FB/50; ISO R306
 99.0 °C210 °FB/120; ISO R306
Flammability, UL94 HB
@Thickness 1.50 - 3.00 mm
HB
@Thickness 0.0591 - 0.118 in
 
Descriptive Properties
Pencil HardnessHB500g, JIS K 5401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-709 ABS
Chi Mei Polylac® PA-707 ABS
Lotte Advanced Materials Starex® LX-0760 ABS
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade
Lotte Advanced Materials Starex® VH-0800 ABS, Unreinforced FR

PSAMSU713 / 146530

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.