MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Starex® BF-0677HF MABS, Unreinforced Scratch Resistant
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifier

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 3.20 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 19 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 114ASTM D785
Tensile Strength at Break 29.4 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 480 kg(f)/cm²5 mm/min; ASTM D638
Elongation at Break 15 %5 mm/min; ASTM D638
Tensile Modulus 24400 kg(f)/cm²5 mm/min; ASTM D638
Flexural Strength 68.6 MPa2.8 mm/min; ASTM D790
Flexural Modulus 25000 kg(f)/cm²2.8 mm/min; ASTM D790
Izod Impact, Notched 9.00 kg-cm/cm
@Thickness 6.35 mm
ASTM D256
 12.0 kg-cm/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point 96.0 °CB/50; ISO R306
 99.0 °CB/120; ISO R306
Flammability, UL94 HB
@Thickness 1.50 - 3.00 mm
 
Descriptive Properties
Pencil HardnessHB500g, JIS K 5401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-709 ABS
Chi Mei Polylac® PA-707 ABS
Lotte Advanced Materials Starex® LX-0760 ABS
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade
Lotte Advanced Materials Starex® VH-0800 ABS, Unreinforced FR

PSAMSU713 / 146530

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.