MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Edinburg Plastics CAT605 PC/ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Appearance: Platable-Paintable Surface Colors

Processing Methods: Injection

Applications: Automotive, Lawn & Garden

Information provided by Edinburg Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792-91
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.2 MPa8000 psiASTM D638
Elongation at Break 110 %110 %ASTM D638
Flexural Yield Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 2.28 GPa330 ksiASTM D790
Izod Impact, Notched 6.41 J/cm12.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 106 °C223 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 238 - 266 °C460 - 511 °F
Middle Barrel Temperature 249 - 277 °C480 - 531 °F
Front Barrel Temperature 260 - 288 °C500 - 550 °F
Nozzle Temperature 266 - 293 °C511 - 559 °F
Melt Temperature 282 °C540 °F
Mold Temperature 71.0 - 99.0 °C160 - 210 °F
Drying Temperature 99.0 °C210 °F
Dry Time 4.00 - 12.0 hour4.00 - 12.0 hour
Moisture Content <= 0.030 %<= 0.030 %
Dew Point >= -40.0 °C>= -40.0 °F
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiLower is better
Screw Speed 30 - 70 rpm30 - 70 rpmLower is better

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Lucent PC/ABS-1211P Polycarbonate+ABS, Impact Modified, Platable, Injection Grade
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Edinburg Plastics CAI406 PC/ABS
Magnesium, Mg; Annealed Sheet
Mitsubishi Chemical Advanced Materials Altron™ PC Extruded, Unfilled, Polycarbonate

PEDIN014 / 183517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.