System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Edinburg Plastics CAT605 PC/ABS
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
Material Notes:
Appearance: Platable-Paintable Surface Colors
Processing Methods: Injection
Applications: Automotive, Lawn & Garden
Information provided by Edinburg Plastics, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.12
g/cc
ASTM D792-91
Linear Mold Shrinkage
0.0050
-
0.0080
cm/cm
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
8000
psi
ASTM D638
Elongation at Break
110 %
ASTM D638
Flexural Yield Strength
12000
psi
ASTM D790
Flexural Modulus
330000
psi
ASTM D790
Izod Impact, Notched
12.0
ft-lb/in
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
106
°C
ASTM D648
Processing Properties
Original Value
Comments
Rear Barrel Temperature
238
-
266
°C
Middle Barrel Temperature
249
-
277
°C
Front Barrel Temperature
260
-
288
°C
Nozzle Temperature
266
-
293
°C
Melt Temperature
282
°C
Mold Temperature
71.0
-
99.0
°C
Drying Temperature
99.0
°C
Dry Time
4.00
-
12.0
hour
Moisture Content
<= 0.030 %
Dew Point
>=
-40.0
°F
Back Pressure
50.0
-
100
psi
Lower is better
Screw Speed
30
-
70
rpm
Lower is better
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
A. Schulman Lucent PC/ABS-1211P Polycarbonate+ABS, Impact Modified, Platable, Injection Grade
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Edinburg Plastics CAI406 PC/ABS
Magnesium, Mg; Annealed Sheet
Mitsubishi Chemical Advanced Materials Altron™ PC Extruded, Unfilled, Polycarbonate
PEDIN014 / 183517
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.