MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott BG64 Bandpass Filter
Categories: Ceramic; Glass; Optical; Filter

Material Notes: IR filter glasses, BG60 – BG64 and BG67, have been designed to perform in difficult environments. Equipped with a specified coating, these filters remain completely transparent for more than 1000 hours without any surface corrosion and deliver extraordinary image quality.

Advantages

  • Repeatable optical performance due to mass production

    Excellent inner quality, e. g. low striae

    Allows true color imaging

    High NIR absorption at smaller thickness

Applications:
  • Medical
  • Imaging
  • Surveillance
  • NVIS (night vision) compatible display
  • Industrial applications

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.78 g/cc0.100 lb/in³
Thickness 100 microns3.94 mil
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 52.352.3
Alkali Class, AR 3.33.3
Stain Resistance Class, FR 1.01.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 371371HK (0.1/20)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.0 µm/m-°C
@Temperature -30.0 - 70.0 °C
6.67 µin/in-°F
@Temperature -22.0 - 158 °F
 13.8 µm/m-°C
@Temperature 20.0 - 300 °C
7.67 µin/in-°F
@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 417 °C783 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.513
@Wavelength 404.7 nm
1.513
@Wavelength 404.7 nm
 1.53
@Wavelength 587.6 nm
1.53
@Wavelength 587.6 nm
 1.532
@Wavelength 546.1 nm
1.532
@Wavelength 546.1 nm
 1.549
@Wavelength 365 nm
1.549
@Wavelength 365 nm
Transmission, Visible  7.0 %
@Wavelength 630 nm
7.0 %
@Wavelength 630 nm
 <= 55 %
@Wavelength 694 nm
<= 55 %
@Wavelength 694 nm
 >= 72 %
@Wavelength 633 nm
>= 72 %
@Wavelength 633 nm
 >= 99 %
@Wavelength 514 nm
>= 99 %
@Wavelength 514 nm
IR Transmittance  <= 0.0010 %
@Wavelength 880 nm
<= 0.0010 %
@Wavelength 880 nm
 <= 8.7 %
@Wavelength >=4150 nm
<= 8.7 %
@Wavelength >=4150 nm
 9.0 %
@Wavelength 2400 - 2800 nm
9.0 %
@Wavelength 2400 - 2800 nm
 9.8 %
@Wavelength 1450 nm
9.8 %
@Wavelength 1450 nm
 <= 45 %
@Wavelength >=1060 nm
<= 45 %
@Wavelength >=1060 nm
UV Transmittance  <= 2.3 %
@Wavelength <=340 nm
<= 2.3 %
@Wavelength <=340 nm
 >= 99 %
@Wavelength 405 nm
>= 99 %
@Wavelength 405 nm
Reflection Coefficient, Visible (0-1) 0.916
@Wavelength 587.6 nm
0.916
@Wavelength 587.6 nm
Reflection Factor P
 
Descriptive Properties
Bubble class2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott N-SF66 Glass
Schott LAK9G15 691548.353, Optical Glass
Schott F2G12 621366.360, Optical Glass
Ohara S-LAH79 Optical Glass
American Computer Optics Water White Filter 2 mm

CSGT9851 / 183104

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.