MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NIZHNEKAMSKNEFTEKHIM 525 General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Grade 525 is a crystal polystyrene for both injection molding and cap layer co-extrusion. Injection molding applications such as medical and laboratory parts, tumblers, and jewel boxes demonstrate the polymer's ability to be molded with minimal stresses and fast cycles. Utilizing 525 as a cap layer in cups, plates and other consumer disposables takes advantage of this polymer's melt rheology.

Information provided by manufacturer

Key Words: PS, CAS Number 9003-53-6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 7.0 - 11 g/10 min
@Load 5.00 kg,
Temperature 200 °C
7.0 - 11 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Chemical PropertiesMetricEnglishComments
Styrene Content <= 0.050 %<= 0.050 %p. 4.10 of the TU
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 37.0 MPa>= 5370 psiASTM D638
Flexural Strength >= 80.0 MPa>= 11600 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point >= 92.0 °C>= 198 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Lucent 6-01 Nylon 6, General Purpose, Injection Grade
Bamberger Polymers Bapolan® 6409 Polystyrene, Injection Grade
Americas Styrenics Styron® 685P Polystyrene
Celanese Nilit FRIANYL A63 S Nylon 6.6 for injection molding
Ineos Nova 4250 High Impact Polystyrene Injection Molding Grade

PNKNH002 / 109269

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.