MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bamberger Polymers Bapolan® 6409 Polystyrene, Injection Grade
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Bapolan PS6409 is designed for injection molding applications requiring superior impact and gloss. It complies with US FDA21 CFR177.1640 and has a 94HB UL rating.

Application: General Purpose.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers.

Key Words: General Purpose; High Gloss; High Impact Resistance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 9.0 g/10 min9.0 g/10 minASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.7 MPa3000 psiASTM D-638
Elongation at Yield 52 %52 %ASTM D-638
Flexural Modulus, 1% Secant 2070 MPa300000 psiASTM D-790A
Izod Impact, Notched 1.34 J/cm2.50 ft-lb/inASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C189 °FASTM D-648
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolan® 6055 Polystyrene, Injection Molding
Ineos Nova 4250 High Impact Polystyrene Injection Molding Grade
A. Schulman Lucent 66-01 Nylon 66, General Purpose, Injection Grade
A. Schulman Lucent 6-01 Nylon 6, General Purpose, Injection Grade
Bamberger Polymers Bapolan® 6050 Polystyrene, Injection Grade

PBP1132 / 191661

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.