MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chengdu Polyster H2040 Thermoplastic Polyether-ester Elastomer (TPEE)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyether Ester Elastomer

Material Notes: Low modulus molding and injection grade. Contains improved color- stable antioxidants. Like H4040, except that heat-ageing resistance is improved. Applications requiring better heat-ageing resistance.

Information provided by Chengdu Polyster Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Melt Flow 7.0 - 9.0 g/10 min7.0 - 9.0 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4040ISO 868
Tensile Strength, Ultimate 25.0 MPa3630 psiISO 527-1
Elongation at Break 530 %530 %ISO 527-1
Flexural Modulus 0.0560 GPa8.12 ksiISO 178
Tear Strength 91.0 kN/m519 pliISO 34
 
Thermal PropertiesMetricEnglishComments
Melting Point 190 °C374 °FISO 3146
Brittleness Temperature -70.0 °C-94.0 °FISO 974

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daplen™ EF040AE TPO Compound
Chengdu Polyster H3303 Thermoplastic Polyether-ester Elastomer (TPEE)
Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE)
Celanese SO.F.TER Sofprene® TPR Standard 36 Foot Ware Compound
Chengdu Polyster H4040 Thermoplastic Polyether-ester Elastomer (TPEE)

PCHEN031 / 79328

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.