MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Xsene® XS10 Orange YCF HDPE, pipe
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: FINATHENE® XS 10 ORANGE YCF is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™.

FINATHENE® XS 10 ORANGE YCF is a high performance compound containing cadmium-free organic pigments. FINATHENE® XS 10 ORANGE YCF is specially developed for gas distribution applications.

FINATHENE® XS 10 ORANGE YCF has a broad bimodal molecular weight distribution that ensures easy processing during extrusion. Due to its high melt strength, FINATHENE® XS 10 ORANGE YCF is particularly suited for extrusion of large diameter, thick wall pipes.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183
Viscosity  270000 cP
@Shear Rate 1000 1/s,
Temperature 190 °C
270000 cP
@Shear Rate 1000 1/s,
Temperature 374 °F
ATOFINA research test
 2.10e+6 cP
@Shear Rate 100 1/s,
Temperature 190 °C
2.10e+6 cP
@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Oxidative Induction Time (OIT) >= 20 min>= 20 min200°C; EN 728
 >= 20 min>= 20 min210°C; EN 728
Melt Flow 0.30 g/10 min
@Load 5.00 kg
0.30 g/10 min
@Load 11.0 lb
ISO 1133
High Load Melt Index 8.0 g/10 min
@Load 21.6 kg
8.0 g/10 min
@Load 47.6 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psiISO 527
Tensile Strength, Yield 26.0 MPa3770 psi
Elongation at Break >= 700 %>= 700 %ISO 527
Elongation at Yield 9.0 %9.0 %ISO 527
Flexural Modulus 1.25 GPa181 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 2.00 J/g-°C0.478 BTU/lb-°FDSC
 2.60 J/g-°C
@Temperature 150 °C
0.621 BTU/lb-°F
@Temperature 302 °F
DSC
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FDIN 52612
 0.200 W/m-K
@Temperature 150 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 302 °F
DIN 52612
Melting Point 130 - 132 °C266 - 270 °Fcrystalline; DSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total 53090 High Density Polyethylene - Blow Molding
Total XSene® 55060 High Density Polyethylene - Blow Molding
Total Xsene® BM 593 HDPE, blow molding
Total XSene® XRC 20 B High Density Polyethylene - Pipes and Fittings
Celanese GUR® 2122 PE-UHMW, Specialty

PFINAP125 / 38708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.