MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Xsene® BM 593 HDPE, blow molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: FINATHENE® BM 593 is a new generation of bimodal high density polyethylene based on hexene (C6) as co-monomer and is produced by the ATOFINA Double Loop Technology™.

FINATHENE® BM 593 has been especially designed for the manufacture of blow molded bottles for aggressive liquids (up to 5 liters). Typical applications are bottles for the packaging of liquid detergents and personal care products.

FINATHENE® BM 593 has a broad (bimodal) molecular weight distribution that ensures easy processing, high machine output and bottles with a good surface finish. Due to the combination of hexene (C6) co-monomer and a bimodal molecular weight distribution, FINATHENE® BM 593 offers an excellent balance between stiffness and environmental stress crack resistance. This ensures a high security of stacking during transit and storage of bottles.

FINATHENE® BM 593 is best processed at temperatures between 180 and 220°C.

Information provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³ISO 1183
Environmental Stress Crack Resistance >= 200 hour>= 200 hourASTM D1693-70
Melt Flow 0.27 g/10 min
@Load 2.16 kg
0.27 g/10 min
@Load 4.76 lb
ISO 1133
High Load Melt Index 26 g/10 min
@Load 21.6 kg
26 g/10 min
@Load 47.6 lb
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 28.0 MPa4060 psiISO 527
Tensile Strength, Yield 31.0 MPa4500 psiISO 527
Elongation at Break >= 700 %>= 700 %ISO 527
Elongation at Yield 7.0 %7.0 %ISO 527
Flexural Modulus 1.55 GPa225 ksiISO 178

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total 53090 High Density Polyethylene - Blow Molding
Total XSene® 55060 High Density Polyethylene - Blow Molding
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
Total 5502 R3 High Density Polyethylene - Blow Molding

PFINAP067 / 38650

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.