MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

North American Western Larch Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Larix occidentalis; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.480 g/cc0.0173 lb/in³Oven Dry Weight/Unseasoned Volume
 0.769 g/cc0.0278 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2000 N450 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2100 N472 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 3700 N832 lb (f)Side
Tensile Strength, Ultimate 1.59 MPa230 psiPerpendicular to Grain*
 3.00 MPa435 psiPerpendicular to Grain
 134 MPa19400 psiAxial
Modulus of Rupture 0.0517 GPa7.50 ksiStatic Bending*
 0.0960 GPa13.9 ksiStatic Bending
Flexural Yield Strength 31.7 MPa4600 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 9.31 GPa1350 ksiStatic Bending*
 13.52 GPa1961 ksiStatic Bending
Compressive Strength 3.86 MPa560 psiPerpendicular to Grain*
 6.80 MPa986 psiPerpendicular to Grain
 22.4 MPa3250 psiParallel to Grain*
 26.2 MPa3800 psiMax Crushing Strength Parallel to Grain*
 56.0 MPa8120 psiParallel to Grain
Poissons Ratio 0.2760.276µLT, 12% Moisture Content
 0.3520.352µTR, 12% Moisture Content
 0.3550.355µLR, 12% Moisture Content
 0.3890.389µRT, 12% Moisture Content
Shear Strength 6.34 MPa920 psiParallel to Grain*
 9.70 MPa1410 psiOrientation Unknown
Impact 3.73.7in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 94009400psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00696 J/cm³1.01 in-lb/in³Static Bending*
Work to Maximum Load 0.0490 J/cm³7.10 in-lb/in³Static Bending*
Toughness 23.8 J17.6 ft-lbRadial
 38.5 J28.4 ft-lbTangential
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.127 W/m-K0.880 BTU-in/hr-ft²-°FOven Dry
 0.159 W/m-K1.10 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.2 %4.2 %Radial; Green to Zero Moisture
 8.1 %8.1 %Tangential; Green to Zero Moisture
 13.2 %13.2 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Red Spruce Wood
American Rocky Mountain Douglas Fir Wood
American Coast Douglas Fir Wood
American White Spruce Wood
Canadian Spruce Wood

PTSA610 / 71268

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.