MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

American Rocky Mountain Douglas Fir Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Marked 'flame-like' growth ring figure. Long lengths and clear grades available. Conifer
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Moderately Durable (10 to 15 years)
Resistance to penetration by preservatives: Resistant/Extremely resistant
Common Applications: Plywood, interior and exterior joinery, construction. Vats and tanks

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Pseudotsuga Menziesii; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.400 g/cc0.0145 lb/in³Oven Dry Weight/Unseasoned Volume
 0.481 g/cc0.0174 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1800 N405 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2000 N450 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 2.41 MPa350 psiPerpendicular to Grain*
Modulus of Rupture 0.0441 GPa6.40 ksiStatic Bending*
Flexural Yield Strength 24.8 MPa3600 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 8.14 GPa1180 ksiStatic Bending*
Compressive Strength 3.10 MPa450 psiPerpendicular to Grain*
 17.4 MPa2520 psiParallel to Grain*
 20.7 MPa3000 psiMax Crushing Strength Parallel to Grain*
Poissons Ratio 0.0290.029µTL, 12% Moisture Content
 0.0360.036µRL, 12% Moisture Content
 0.2920.292µLR, 12% Moisture Content
 0.3740.374µTR, 12% Moisture Content
 0.390.39µRT, 12% Moisture Content
 0.4490.449µLT, 12% Moisture Content
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 6.07 MPa880 psiParallel to Grain*
Impact 3.03.0in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 91009100psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00448 J/cm³0.650 in-lb/in³Static Bending*
Work to Maximum Load 0.0469 J/cm³6.80 in-lb/in³Static Bending*
 
Thermal PropertiesMetricEnglishComments
Shrinkage 2.8 %2.8 %Radial; Unseasoned to Oven Dry*
 6.6 %6.6 %Tangential; Unseasoned to Oven Dry*
 10.3 %10.3 %Volumetric; Unseasoned to Oven Dry*
 
Descriptive Properties
ColorLight reddish-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Coast Douglas Fir Wood
American Red Spruce Wood
Interior North Douglas Fir Wood
Interior West Douglas Fir Wood
Douglas-fir Plywood

PTSA560 / 71263

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.