Chromium-molybdenum-vanadium alloyed steel QRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum, copper and brass. QRO® 90 SUPREME is characterized by: - Excellent high temperature strength and hot hardness
- Very good temper resistance
- Unique resistance to thermal fatigue
- Excellent thermal conductivity
- Good toughness and ductility in longitudinal and transverse directions
- Uniform machinability
- Good heat treatment properties
Applications: Die Casting Dies and Associated Tooling, Extrusion dies and Extrusion Tooling and Forging dies |