MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Orbilan RubberLen® 55 HMW-PE, dark blue
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: ORBILAN RUBBERLEN® is a two-layered laminated panel made from Thermoplastic Elastomer (TPE) and low-pressure Polyethylene of High Molecular Weight (HMW-PE). RUBBERLEN® distinguishes itself by very good vibration damping and noise reduction. These properties are highly regarded for applications in the area of lining.

Information provided by the manufacturer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183
Water Absorption <= 0.010 %<= 0.010 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °Fcontinuous
Minimum Service Temperature, Air -40.0 °C-40.0 °Fcontinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Okulen® 500 PE-HMW, UV - stabilized
Orbilan ORBILAN® PE 500 HMW-PE
Dow HMW 2220 Non-Ionic Emulsion
Dow BETAPHON™ 2 Synthetic Rubber
Dow BETADAMP™ 24 Vibration Damper

PORBIL03 / 55705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.