MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 6, Nucleated
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Nucleated

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.41 g/cc0.0397 - 0.0509 lb/in³Average value: 1.14 g/cc Grade Count:90
Water Absorption 1.50 - 9.50 %1.50 - 9.50 %Average value: 2.80 % Grade Count:52
Moisture Absorption at Equilibrium 0.250 - 3.00 %0.250 - 3.00 %Average value: 2.85 % Grade Count:29
Water Absorption at Saturation 8.00 - 10.0 %8.00 - 10.0 %Average value: 9.18 % Grade Count:48
Water Vapor Transmission 10.1 - 35.0 g/m²/day0.650 - 2.25 g/100 in²/dayAverage value: 21.7 g/m²/day Grade Count:15
Oxygen Transmission 1.00 - 70.0 cc-mm/m²-24hr-atm2.54 - 178 cc-mil/100 in²-24hr-atmAverage value: 21.4 cc-mm/m²-24hr-atm Grade Count:15
Carbon Dioxide Transmission 80.0 - 250 cc-mm/m²-24hr-atm203 - 635 cc-mil/100 in²-24hr-atmAverage value: 141 cc-mm/m²-24hr-atm Grade Count:9
Viscosity 810 - 810000 cP
@Temperature 260 - 260 °C
810 - 810000 cP
@Temperature 500 - 500 °F
Average value: 7770 cP Grade Count:6
 40.0 - 2500 cP
@Temperature 240 - 280 °C
40.0 - 2500 cP
@Temperature 464 - 536 °F
Average value: 7770 cP Grade Count:6
 40.0 - 2500 cP
@Shear Rate 0.100 - 10000 1/s
40.0 - 2500 cP
@Shear Rate 0.100 - 10000 1/s
Average value: 7770 cP Grade Count:6
Viscosity Test 120 - 263 cm³/g1.20 - 2.63 dl/gAverage value: 167 cm³/g Grade Count:17
Viscosity Number 195 - 245 cm³/g1.95 - 2.45 dl/gAverage value: 217 cm³/g Grade Count:6
Linear Mold Shrinkage 0.00130 - 0.0200 cm/cm0.00130 - 0.0200 in/inAverage value: 0.0113 cm/cm Grade Count:57
 0.00800 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
0.00800 - 0.00800 in/in
@Temperature 176 - 176 °F
Average value: 0.00800 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00700 - 0.0200 cm/cm0.00700 - 0.0200 in/inAverage value: 0.00987 cm/cm Grade Count:31
 0.00900 - 0.00900 cm/cm
@Temperature 80.0 - 80.0 °C
0.00900 - 0.00900 in/in
@Temperature 176 - 176 °F
Average value: 0.00900 cm/cm Grade Count:2
Melt Flow 8.00 - 260 g/10 min8.00 - 260 g/10 minAverage value: 76.6 g/10 min Grade Count:33
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100 - 120100 - 120Average value: 115 Grade Count:13
Ball Indentation Hardness 55.0 - 150 MPa7980 - 21800 psiAverage value: 98.7 MPa Grade Count:7
Tensile Strength, Ultimate 40.0 - 100 MPa5800 - 14500 psiAverage value: 67.1 MPa Grade Count:34
Film Tensile Strength at Yield, MD 34.0 - 40.0 MPa4930 - 5800 psiAverage value: 36.0 MPa Grade Count:14
Film Tensile Strength at Yield, TD 30.0 - 40.0 MPa4350 - 5800 psiAverage value: 35.6 MPa Grade Count:8
Tensile Strength, Yield 36.0 - 90.3 MPa5220 - 13100 psiAverage value: 68.8 MPa Grade Count:38
Film Elongation at Break, MD 350 - 700 %350 - 700 %Average value: 514 % Grade Count:14
Film Elongation at Break, TD 700 - 900 %700 - 900 %Average value: 813 % Grade Count:8
Film Elongation at Yield, MD 10.0 - 15.0 %10.0 - 15.0 %Average value: 11.9 % Grade Count:8
Film Elongation at Yield, TD 7.00 - 15.0 %7.00 - 15.0 %Average value: 10.0 % Grade Count:8
Elongation at Break 3.00 - 240 %3.00 - 240 %Average value: 51.8 % Grade Count:57
Elongation at Yield 2.50 - 35.0 %2.50 - 35.0 %Average value: 12.3 % Grade Count:37
Modulus of Elasticity 0.400 - 5.70 GPa58.0 - 827 ksiAverage value: 2.08 GPa Grade Count:67
Flexural Yield Strength 9.65 - 150 MPa1400 - 21800 psiAverage value: 83.3 MPa Grade Count:46
 30.0 - 30.0 MPa
@Temperature 90.0 - 90.0 °C
4350 - 4350 psi
@Temperature 194 - 194 °F
Average value: 30.0 MPa Grade Count:1
Flexural Modulus 0.800 - 4.80 GPa116 - 696 ksiAverage value: 2.32 GPa Grade Count:49
 0.600 - 0.600 GPa
@Temperature 90.0 - 90.0 °C
87.0 - 87.0 ksi
@Temperature 194 - 194 °F
Average value: 0.600 GPa Grade Count:1
Izod Impact, Notched 0.400 - 6.41 J/cm0.749 - 12.0 ft-lb/inAverage value: 1.18 J/cm Grade Count:21
 3.2034 - 4.53815 J/cm
@Temperature -40.0 - -20.0 °C
6.0013 - 8.50182 ft-lb/in
@Temperature -40.0 - -4.00 °F
Average value: 3.87 J/cm Grade Count:2
 3.2034 - 4.53815 J/cm
@Thickness 3.17 - 3.17 mm
6.0013 - 8.50182 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 3.87 J/cm Grade Count:2
Izod Impact, Notched (ISO) 2.94 - 100000 kJ/m²1.40 - 47600 ft-lb/in²Average value: 4.06 kJ/m² Grade Count:9
 3.00 - 3.50 kJ/m²
@Temperature -40.0 - -30.0 °C
1.43 - 1.67 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 3.25 kJ/m² Grade Count:2
Charpy Impact Unnotched 4.30 J/cm² - NB20.5 ft-lb/in² - NBAverage value: 16.2 J/cm² Grade Count:39
 2.94 - 2099.79 J/cm²
@Temperature -30.0 - -30.0 °C
14.0 - 9993.41 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 14.5 J/cm² Grade Count:11
Charpy Impact, Notched 0.294 J/cm² - NB1.40 ft-lb/in² - NBAverage value: 1.55 J/cm² Grade Count:40
 0.294 - 3.00 J/cm²
@Temperature -30.0 - -30.0 °C
1.40 - 14.3 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.542 J/cm² Grade Count:16
Coefficient of Friction 0.250 - 0.8000.250 - 0.800Average value: 0.515 Grade Count:13
Coefficient of Friction, Static 1.401.40Average value: 1.40 Grade Count:6
Tear Strength Test 32.0 - 28632.0 - 286Average value: 185 Grade Count:14
Elmendorf Tear Strength MD 998 - 1540 g998 - 1540 gAverage value: 1340 g Grade Count:8
Elmendorf Tear Strength TD 998 - 1540 g998 - 1540 gAverage value: 1340 g Grade Count:8
Film Tensile Strength at Break, MD 94.0 - 100 MPa13600 - 14500 psiAverage value: 97.8 MPa Grade Count:13
Film Tensile Strength at Break, TD 90.3 MPa13100 psiAverage value: 90.3 MPa Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+8 - 1.00e+17 ohm-cm1.00e+8 - 1.00e+17 ohm-cmAverage value: 4.72e+15 ohm-cm Grade Count:46
Surface Resistance 1.00e+7 - 1.00e+15 ohm1.00e+7 - 1.00e+15 ohmAverage value: 1.32e+14 ohm Grade Count:29
Dielectric Constant 3.00 - 8.003.00 - 8.00Average value: 4.93 Grade Count:22
Dielectric Strength 5.12 - 31.9 kV/mm130 - 810 kV/inAverage value: 19.7 kV/mm Grade Count:27
Dissipation Factor 0.00300 - 0.1000.00300 - 0.100Average value: 0.0513 Grade Count:4
Comparative Tracking Index 550 - 600 V550 - 600 VAverage value: 598 V Grade Count:32
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 - 108 µm/m-°C3.89 - 60.0 µin/in-°FAverage value: 65.4 µm/m-°C Grade Count:32
 80.0 - 80.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
44.4 - 44.4 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 80.0 µm/m-°C Grade Count:1
 80.0 - 80.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
44.4 - 44.4 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 80.0 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 50.4 - 101 µm/m-°C28.0 - 56.0 µin/in-°FAverage value: 91.7 µm/m-°C Grade Count:15
Specific Heat Capacity 1.55 - 2.25 J/g-°C0.370 - 0.538 BTU/lb-°FAverage value: 1.90 J/g-°C Grade Count:6
Melting Point 215 - 222 °C419 - 432 °FAverage value: 221 °C Grade Count:38
Maximum Service Temperature, Air 65.0 - 180 °C149 - 356 °FAverage value: 128 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 160 - 197 °C320 - 387 °FAverage value: 181 °C Grade Count:32
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 195 °C122 - 383 °FAverage value: 71.4 °C Grade Count:42
Vicat Softening Point 190 - 215 °C374 - 419 °FAverage value: 201 °C Grade Count:7
Minimum Service Temperature, Air 70.0 - 100 °C158 - 212 °FAverage value: 76.0 °C Grade Count:5
Flammability, UL94 HB - V-0HB - V-0Grade Count:33
Oxygen Index 23.0 - 32.0 %23.0 - 32.0 %Average value: 26.0 % Grade Count:6
Glow Wire Test 700 - 900 °C1290 - 1650 °FAverage value: 787 °C Grade Count:9
 
Optical PropertiesMetricEnglishComments
Gloss 100 %100 %Average value: 100 % Grade Count:9
Transmission, Visible 85.0 %85.0 %Average value: 85.0 % Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 295 °C446 - 563 °FAverage value: 268 °C Grade Count:10
Nozzle Temperature 227 - 293 °C440 - 560 °FAverage value: 254 °C Grade Count:5
Die Temperature 270 °C518 °FAverage value: 270 °C Grade Count:6
Melt Temperature 216 - 300 °C420 - 572 °FAverage value: 256 °C Grade Count:34
Mold Temperature 21.1 - 120 °C70.0 - 248 °FAverage value: 66.9 °C Grade Count:34
Roll Temperature 110 °C230 °FAverage value: 110 °C Grade Count:6
Drying Temperature 73.9 - 100 °C165 - 212 °FAverage value: 80.2 °C Grade Count:34
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.164 % Grade Count:6
Injection Pressure 34.5 - 172 MPa5000 - 25000 psiAverage value: 99.6 MPa Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Heat Stabilized
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 6, Extruded
Overview of materials for Nylon 6, Impact Grade
Overview of materials for Nylon 6, Film Grade

O2407 / 77968

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.