MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AK Steel 420 ULTRA HONE® Martensitic Stainless steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximum corrosion resistance is attained only in the fully hardened of fully hardened and stress relieved condition. It is never used in the annealed condition. Typical uses include cutlery, surgical and dental instruments, scissors, tapes and straight edges. The alloy is not normally used at temperatures exceeding 800°F due to rapid softening and loss of corrosion resistance.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.74 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8888Annealed
Hardness, Rockwell C 5555Hardened and Stress Relieved
Tensile Strength, Ultimate 586 MPa85000 psiAnnealed
 1586 MPa230000 psiHardened and Stress Relieved
Tensile Strength, Yield  276 MPa
@Strain 0.2 %
40000 psi
@Strain 0.2 %
Annealed
 1344 MPa
@Strain 0.2 %
194900 psi
@Strain 0.2 %
Hardened and Stress Relieved
Elongation at Break 8.0 %8.0 %in 2 inches, Hardened and Stress Relieved
 25 %25 %in 2 inches, Annealed
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000550 ohm-cm0.0000550 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.2 µm/m-°C
@Temperature 0.000 - 100 °C
5.67 µin/in-°F
@Temperature 32.0 - 212 °F
 12.1 µm/m-°C
@Temperature <=649 °C
6.72 µin/in-°F
@Temperature <=1200 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 24.9 W/m-K173 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C >= 0.15 %>= 0.15 %
Chromium, Cr 12 - 14 %12 - 14 %
Iron, Fe 83.78 - 87.85 %83.78 - 87.85 %As Remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
420 Stainless Steel
AK Steel 420 Martensitic Stainless steel
420 Stainless Steel, hardened and tempered bar
420 Stainless Steel, annealed and cold drawn bar
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420

NAKS104c / 140578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.