MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC AFLAS® 150CS TFE/P Latex
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: AFLAS 150CS Latex is an alternating tetrafluoroethylene–propylene copolymer in an aqueous suspension. It is used as an elastomeric surface treatment of various substrates such as metals, ceramics, plastics, other elastomers, textiles, and paper. Classified by ASTM D 1418-01 as FEPM.

Material Features:

    Heat Resistance*: Mechanical properties of AFLAS do not deteriorate even when used for prolonged exposure to 200°C. AFLAS can be used continuously for 2 to 3 months at 230°C and for 10-30 days at 260°C.
  • Chemical Resistance: Parts fabricated from AFLAS compounds perform well in the amine and base-rich environments commonly found in sour oil and gas exploration, completion and production. In automotive and heavy equipment applications, AFLAS stands up well to attack from amine-containing additives in oils and transmission fluids.
  • Steam Resistance*: Unaffected by extended exposure to 200°C steam.
  • Electrical Properties: Excellent volume resistivity (greater than 1016 O-cm) unmatched by other fluoroelastomers.
  • Radiation Resistance*: Stable up to 200 MRad of gamma ray radiation.
End User Benefits:
    Improved flexibility
  • Excellent thermal and chemical stability
  • Water and weather resistant
Typical Applications:
    Binder
  • Coating additives
  • Surface modified parts

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 - 1.20 g/cc1.05 - 1.20 g/cc
Solids Content 30 - 35 %30 - 35 %
Particle Size 50 - 200 µm50 - 200 µm
pH 7.0 - 9.07.0 - 9.0
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 230 °C446 °F
 260 °C500 °F
 
Descriptive Properties
AppearanceWhite, milky liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC AFLAS® 150L TFE/P Fluoroelastomers
AGC AFLAS® PM-3000 TFE/P Perfluoroelastomer
AGC AFLAS® 300S TFE/P Latex
AGC AFLAS® 200P TFE/P Fluoroelastomers
AGC AFLAS® 150P TFE/P Fluoroelastomers

PAGCX004 / 191113

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.