MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC AFLAS® 200P TFE/P Fluoroelastomers
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: AFLAS® 200P (SPL-FKM) is a peroxide-curable specialty fluoroelastomer offering improved performance over conventional FKM-type fluoroelastomers in demanding applications found in the oil & gas, chemical process, industrial equipment, food handling, pharmaceutical, heavy duty diesel and automotive industries. AFLAS® 200P displays outstanding resistance to heat, acids & bases, many solvents, and ozone. Classified by ASTM D 1418-01 as TYPE IV FKM

Material Features:

    Improved cold temperature performance (Tg = -13°C, TR-10 = -8°C)
  • Retains good base resistance and heat tolerance
  • Can be solvated and applied as a coating
End User Benefits:
    Longer life of seals
  • Resists aggressive oils which contain anti-oxidants
  • Improved sealing for cold application environments
Typical Applications:
    Oil seals
  • Shaft seals
  • O-Rings
  • Gaskets

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity  65
@Temperature 121 °C
65
@Temperature 250 °F
[kN/m], (ML1+10)
 90
@Temperature 100 °C
90
@Temperature 212 °F
[kN/m], (ML1+10)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.0 MPa2610 psi
 15.12 MPa
@Treatment Temp. 70.0 °C,
Time 2.59e+6 sec
2193 psi
@Treatment Temp. 158 °F,
Time 720 hour
28% Aq Ammonia Resistance
 16.2 MPa
@Treatment Temp. 200 °C,
Time 3.60e+6 sec
2350 psi
@Treatment Temp. 392 °F,
Time 1000 hour
Heat Resistance
 17.1 MPa
@Treatment Temp. 175 °C,
Time 2.59e+6 sec
2480 psi
@Treatment Temp. 347 °F,
Time 720 hour
Engine Oil (SM class) Resistance
 17.64 MPa
@Treatment Temp. 70.0 °C,
Time 2.59e+6 sec
2558 psi
@Treatment Temp. 158 °F,
Time 720 hour
50% NaOH aq Resistance
Elongation at Break 270 %270 %
 167.4 %
@Treatment Temp. 70.0 °C,
Time 2.59e+6 sec
167.4 %
@Treatment Temp. 158 °F,
Time 720 hour
28% Aq Ammonia Resistance
 194.4 %
@Treatment Temp. 175 °C,
Time 2.59e+6 sec
194.4 %
@Treatment Temp. 347 °F,
Time 720 hour
Engine Oil (SM class) Resistance
 194.4 %
@Treatment Temp. 200 °C,
Time 3.60e+6 sec
194.4 %
@Treatment Temp. 392 °F,
Time 1000 hour
Heat Resistance
 240.3 %
@Treatment Temp. 70.0 °C,
Time 2.59e+6 sec
240.3 %
@Treatment Temp. 158 °F,
Time 720 hour
50% NaOH aq Resistance
Tensile Modulus 0.000220 GPa0.0319 ksiG' Storage Modulus (nominal) of Raw Gum
100% Modulus 5.00 MPa
@Strain 100 %
725 psi
@Strain 100 %
Compression Set 23 %
@Temperature 200 °C,
Time 252000 sec
23 %
@Temperature 392 °F,
Time 70.0 hour
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -13.0 °C8.60 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  1.70 min
@Temperature 150 °C
0.0283 hour
@Temperature 302 °F
10% Cure, 100CPM, 3° Strain, 12 minutes by RPA-2000
 6.50 min
@Temperature 150 °C
0.108 hour
@Temperature 302 °F
90% Cure, 100CPM, 3° Strain, 12 minutes by RPA-2000
 20.0 min
@Temperature 170 °C
0.333 hour
@Temperature 338 °F
Press Cure
 1440 min
@Temperature 230 °C
24.0 hour
@Temperature 446 °F
Post cure
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 60 %60 %
 
Descriptive Properties
Cure Data61.4 dNmMax S'
 7.7 dNmMin S'
Volume Change (%)150% NaOH aq Resistance 70°C for 720 hours
 3Engine Oil (SM class) Resistance 175°C for 720 hours
 3228% Aq Ammonia Resistance 70°C for 720 hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC AFLAS® 150L TFE/P Fluoroelastomers
AGC AFLAS® 100S TFE/P Fluoroelastomers
AGC AFLAS® 100H TFE/P Fluoroelastomers
AGC AFLAS® PM-1100 TFE/P Perfluoroelastomer
AGC AFLAS® 300S TFE/P Latex

PAGCX006 / 191115

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.